Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.00 - 12.0 J/cm² @Thickness 4.0 mm |
19.0 - 57.1 ft-lb/in² @Thickness 0.16 in |
MD; ISO 179-12fn / PA_097 |
Quadrant Plastic Composites GMT Glass-Mat-Reinforced Thermoplastic This semi-finished product in panel form was developed primarily as a substitute for metals (steel, aluminum etc.) and its main purchasers can be found in the automotive industry. This is where it i.. |
|||
Charpy Impact Unnotched | 0.800 - 12.0 J/cm² | 3.81 - 57.1 ft-lb/in² | Average value: 4.03 J/cm² Grade Count:95 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact Unnotched | 7.00 - 12.0 J/cm² @Temperature -30.0 - -30.0 °C |
33.3 - 57.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 8.60 J/cm² Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 12.0 - 12.0 J/cm² @Temperature -30.0 - -30.0 °C |
57.1 - 57.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 12.0 J/cm² Grade Count:1 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact Unnotched | 5.00 - 12.0 J/cm² | 23.8 - 57.1 ft-lb/in² | Average value: 8.23 J/cm² Grade Count:15 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact Unnotched | 2.50 - 12.0 J/cm² @Temperature -40.0 - -20.0 °C |
11.9 - 57.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.81 J/cm² Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |