Mechanical Properties Metric English Comments
Charpy Impact Unnotched 22.2 J/cm²

@Temperature -30.0 °C
106 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Kynar® 4000 HD PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b..