Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.2 J/cm² @Temperature -30.0 °C |
48.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4271 PC Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² @Temperature -30.0 °C |
48.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² | 48.5 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Charpy Impact Unnotched | 10.2 J/cm² @Temperature -30.0 °C |
48.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, Conditioned Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² | 48.5 ft-lb/in² | ISO 179/1eU |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² | 48.5 ft-lb/in² | ISO 179-1 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 10.2 J/cm² | 48.5 ft-lb/in² | |
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² @Temperature 23.0 °C |
48.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² | 48.5 ft-lb/in² | ISO 179 |
BASF Ultramid® B3ZG7 OSI BK23273 35% Glass Filled PA6 (Dry) Ultramid B3ZG7 OSI BK23273 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet demanding mechanical and chemical requi.. |
|||
Charpy Impact Unnotched | 10.2 J/cm² @Temperature -30.0 °C |
48.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |