Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.96 - 3.74 J/cm² | 9.33 - 17.8 ft-lb/in² | Average value: 2.90 J/cm² Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact Unnotched | 1.96 J/cm² @Temperature 23.0 °C |
9.33 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact Unnotched | 1.96 J/cm² @Temperature -30.0 °C |
9.33 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned) Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No .. |