Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink 220A RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink RP - rephosphorized steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.5 - 1.5 mm. Iron content is approximate - exact compo.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink 260A RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink RP - rephosphorized steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.5 - 1.5 mm. Iron content is approximate - exact compo.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink 280A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink 350A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink 420A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink B420A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink B500A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink F26A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bending; avoid bending and rebending |
SSAB Tunnplat Aluzink F30A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t = 1.5 mm |
SSAB Tunnplat Docol® 600DL High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 90° bend |
SSAB Tunnplat Docol® 800 DL High-strength Steel In course of development.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t = 1.0 mm |
SSAB Tunnplat Docol® 800 DP High-strength Steel Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm.Data provided by SSAB Tunnplat. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 420MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t>6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 420MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 460MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 490XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 500MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 550MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 600MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 640XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 650MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 690XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 700MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.0 t | >= 1.0 t | t<3mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 740XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Bend Radius, Minimum | 1.0 t | 1.0 t | ISO 7438 |
ThyssenKrupp PAS 460 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Bend Radius, Minimum | 1.0 t | 1.0 t | ISO 7438 |
ThyssenKrupp PAS 500 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |