Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.798 J/cm² @Temperature -30.0 °C |
3.80 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F.. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature -20.0 °C |
3.80 ft-lb/in² @Temperature -4.00 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior .. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature -20.0 °C |
3.80 ft-lb/in² @Temperature -4.00 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 139 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature 0.000 °C |
3.80 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 143 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature 0.000 °C |
3.80 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 143S Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive interior application in which good surface finish, hig.. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature -30.0 °C |
3.80 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ H1725W Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with very high flow. Product presenting very high rigidity, maintaining excellent impact resistance properties, including at a low tem.. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature 0.000 °C |
3.80 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature 22.8 °C |
3.80 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Charpy Impact, Notched | 0.798 J/cm² @Temperature 22.8 °C |
3.80 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil PPU0009F Polypropylene Impact Copolymer Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobi.. |