Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.441 J/cm² @Temperature -20.0 °C |
2.10 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
ExxonMobil Exxtral™ BMU 141 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s.. |
|||
Charpy Impact, Notched | 0.441 J/cm² @Temperature -30.0 °C |
2.10 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability.. |
|||
Charpy Impact, Notched | 0.441 J/cm² @Temperature -30.0 °C |
2.10 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea.. |
|||
Charpy Impact, Notched | 0.441 J/cm² @Temperature -20.0 °C |
2.10 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
ExxonMobil Exxtral™ CNR 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and Nort.. |
|||
Charpy Impact, Notched | 0.441 J/cm² @Temperature -30.0 °C |
2.10 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CNU 015 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & M.. |
|||
Charpy Impact, Notched | 0.441 J/cm² @Temperature -20.0 °C |
2.10 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil PP7011L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets .. |
|||
Charpy Impact, Notched | 0.441 J/cm² @Temperature -20.0 °C |
2.10 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil PP7064L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain.. |