Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nyco NYLITE® Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYLITE® Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3) is a natur.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radiflam® A RV250FR (dry) Nylon 66-25GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radiflam® S AE (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® S AE (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S CP400 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 22.8 °C |
2.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature 0.000 °C |
2.00 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Charpy Impact, Notched | 0.420 J/cm² @Temperature -30.0 °C |
2.00 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |