Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.315 J/cm² @Temperature 0.000 °C |
1.50 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMU 201 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness toughness balance is required.Availa.. |
|||
Charpy Impact, Notched | 0.315 J/cm² @Temperature 0.000 °C |
1.50 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMV 205 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance .. |
|||
Charpy Impact, Notched | 0.315 J/cm² @Temperature -30.0 °C |
1.50 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |