Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 81 T 15 PP, 15% mineral filling FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 104 PC (Europe-Africa-Middle East) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL6033 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with good processability.Very low temp. ductility, UV-Stabilized, UL94 V1 rated in white colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD951A PC Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE101R PC (Europe-Africa-Middle East) Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7690 PC (Europe-Africa-Middle East) LEXAN ML7690 is a high viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN ML7690 is available in transparent, translucent and opaque colours... |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BTQ80-AQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature -30.0 °C |
35.7 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 179-1eA |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Pocan® S 1506 901510 PBT PBT, injection molding grade, non-reinforced, elastomer-modified, high impact strength, even at low temperatures |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Thickness 3.00 mm, Temperature 23.0 °C |
35.7 ft-lb/in² @Thickness 0.118 in, Temperature 73.4 °F |
partial break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66 Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K223-TP4 (Cond.) Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 7.50 J/cm² @Temperature 23.0 °C |
35.7 ft-lb/in² @Temperature 73.4 °F |
partial break; DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding.. |