Polymer Property : Charpy Impact, Notched = 4.80 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.80 J/cm²

@Temperature -20.0 °C
22.8 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® PQ 81 T 15/1 Polypropylene reinforced with mineral filler, impact modified
Modified PP for injection molding with the content of 15% mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o.
Charpy Impact, Notched 4.80 J/cm²

@Temperature -20.0 °C
22.8 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PQ 81 T 15 PP, 15% mineral filling
FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene..
Charpy Impact, Notched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
Charpy Impact, Notched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according ..
Charpy Impact, Notched 4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Eurotec® Tecomid® NB40 NL IL PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..