Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.609 J/cm² @Temperature -30.0 °C |
2.90 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 131 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, good surface appearance and good weatherability designed for automotive exterior .. |
|||
Charpy Impact, Notched | 0.609 J/cm² @Temperature 22.8 °C |
2.90 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMV 205 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance .. |
|||
Charpy Impact, Notched | 0.609 J/cm² @Temperature -5.00 °C |
2.90 ft-lb/in² @Temperature 23.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CNU 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and Nor.. |
|||
Charpy Impact, Notched | 0.609 J/cm² @Temperature 0.000 °C |
2.90 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil PP7011L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets .. |