Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.546 J/cm² @Temperature -30.0 °C |
2.60 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMT222 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by good stiffness/toughness balance and designed for automotive interior applications in which good surface finish and g.. |
|||
Charpy Impact, Notched | 0.546 J/cm² @Temperature -30.0 °C |
2.60 ft-lb/in² @Temperature -22.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 133 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for paintable automotive exterior applications.Availability: Europe .. |
|||
Charpy Impact, Notched | 0.546 J/cm² @Temperature -20.0 °C |
2.60 ft-lb/in² @Temperature -4.00 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea.. |
|||
Charpy Impact, Notched | 0.546 J/cm² @Temperature 0.000 °C |
2.60 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |
|||
Charpy Impact, Notched | 0.546 J/cm² @Temperature 0.000 °C |
2.60 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac.. |
|||
Charpy Impact, Notched | 0.546 J/cm² @Temperature 0.000 °C |
2.60 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil PP7064L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, contain.. |