Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179
ExxonMobil Exxtral™ BMU 141 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s..
Charpy Impact, Notched 0.441 J/cm²

@Temperature -30.0 °C
2.10 ft-lb/in²

@Temperature -22.0 °F
ISO 179
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability..
Charpy Impact, Notched 0.441 J/cm²

@Temperature -30.0 °C
2.10 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea..
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179
ExxonMobil Exxtral™ CNR 012 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and Nort..
Charpy Impact, Notched 0.441 J/cm²

@Temperature -30.0 °C
2.10 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNU 015 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & M..
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets ..
Charpy Impact, Notched 0.441 J/cm²

@Temperature -20.0 °C
2.10 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
ExxonMobil PP7064L1 Polypropylene Impact Copolymer