Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Nyco NYLITE® Wollastonite in Polypropylene
Data for polypropylene reinforced with 15% Nyco NYLITE® Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3) is a natur..
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® A RV250FR (dry) Nylon 66-25GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® S AE (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® S AE (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S CP400 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.420 J/cm²

@Temperature 22.8 °C
2.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated
General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized
50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
Charpy Impact, Notched 0.420 J/cm²

@Temperature 0.000 °C
2.00 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
ExxonMobil AP03B Polypropylene Impact Copolymer
Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol..