| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 1200-15 Polycarbonate Resin
Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 3010-15 Polycarbonate Resin
Description: LUPOY PC 3010-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 3030-15 Polycarbonate Resin
Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
|
|||
| Izod Impact, Notched |
8.541
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
16.00
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
0.25 mm notch; ASTM D256 |
|
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
|
|||