Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 13.00 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.941 J/cm
13.00 ft-lb/in
ASTM D256
Ovation Polymers RIGITRON 10001 Polycarbonate
PC – Impact Modified, high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to..
Izod Impact, Notched 6.939 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
13.00 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1301EP30 Polycarbonate Resin
Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Izod Impact, Notched 6.939 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
13.00 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin
Description: LUPOY PC 1302EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Izod Impact, Notched 6.939 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
13.00 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin
Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Izod Impact, Notched 6.939 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
13.00 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
0.25 mm notch; ASTM D256
LG Chemical Lupoy 3010-30 Polycarbonate Resin
Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..