Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 - 4.50 J/cm | 0.599 - 8.43 ft-lb/in | Average value: 0.658 J/cm Grade Count:44 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.135 - 4.50 J/cm | 0.253 - 8.43 ft-lb/in | Average value: 0.940 J/cm Grade Count:178 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |