Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.750 - 1.50 J/cm | 1.41 - 2.81 ft-lb/in | Average value: 1.05 J/cm Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Notched | 0.450 - 1.50 J/cm @Temperature -40.0 - 0.000 °C |
0.843 - 2.81 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.579 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.550 - 1.50 J/cm | 1.03 - 2.81 ft-lb/in | Average value: 1.04 J/cm Grade Count:4 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Izod Impact, Notched | 0.900 - 1.50 J/cm | 1.69 - 2.81 ft-lb/in | Average value: 1.18 J/cm Grade Count:4 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Izod Impact, Notched | 1.30 - 1.50 J/cm | 2.44 - 2.81 ft-lb/in | ASTM D256 |
Loxim 130 01HB Polycarbonate, 30% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.30 - 1.50 J/cm | 2.44 - 2.81 ft-lb/in | ASTM D256 |
Loxim 130 01V0 Polycarbonate, 30% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.380 - 1.50 J/cm @Temperature -40.0 - -20.0 °C |
0.712 - 2.81 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.940 J/cm Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |