Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.420 - 1.28 J/cm
0.787 - 2.40 ft-lb/in
Average value: 0.679 J/cm Grade Count:53
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched 0.214 - 1.28 J/cm
0.400 - 2.40 ft-lb/in
Average value: 0.364 J/cm Grade Count:16
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Izod Impact, Notched 0.160 - 1.28 J/cm
0.300 - 2.40 ft-lb/in
Average value: 0.506 J/cm Grade Count:27
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched 0.427 - 1.28 J/cm
0.800 - 2.40 ft-lb/in
Average value: 0.843 J/cm Grade Count:34
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 1.07 - 1.28 J/cm
2.00 - 2.40 ft-lb/in
ASTM D265
Alcoa KAMA 3200 Prime High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea..
Izod Impact, Notched 0.801 - 1.28 J/cm
1.50 - 2.40 ft-lb/in
Average value: 0.949 J/cm Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..