Polymer Property : Izod Impact, Notched = 7.53 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.02 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
7.53 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HI110 ABS, High Impact, Chemical Resistance
Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 4.02 J/cm

@Thickness 6.35 mm
7.53 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.02 J/cm
7.53 ft-lb/in
ASTM D256
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic
SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo..
Izod Impact, Notched 4.02 J/cm

@Thickness 6.35 mm
7.53 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.