Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.26 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
6.10 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® AS-1000 HI Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:High ImpactPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 3.26 J/cm | 6.10 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Pro-faxâ„¢ SR257M Polypropylene Copolymer Description: Pro-faxâ„¢ SR257M clarified polypropylene random copolymer resin has excellent see-through and contact clarity. This resin offers source reduction potential in blow molding and extru.. |