Polymer Property : Izod Impact, Notched = 4.18 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.23 J/cm
4.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL NH7010 PPE+PS
Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts..
Izod Impact, Notched 2.23 J/cm
4.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific)
High heat, Non halogenated flame retardant Noryl product
Izod Impact, Notched 2.23 J/cm
4.18 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific)
Low odor grade for IC tray application