Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.20 mm |
3.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.20 mm |
3.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
NOVA Chemicals Novapol® TR-0338-U MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare. |
|||
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM Data |
Dow C702-20 Polypropylene Impact Copolymer Dow Polypropylene Impact Copolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resis.. |
|||
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 261WO PPO A general purpose V-0 rated resin with good impact strength.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LD-33G Nylon 66, High Impact, 33% Glass Reinforced A high impact reinforced Nylon 66 with good low temperature properties.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 559LD-33G Nylon 66, 33% Glass Reinforced A high impact reinforced nylon copolymer with good low temperature properties.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.82 J/cm | 3.41 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 727 Nylon 6 A modified nylon for applications requiring flexibility.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.20 mm |
3.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |