Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.74746 - 0.74746 J/cm @Temperature -40.0 - -40.0 °C |
1.4003 - 1.4003 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.747 J/cm Grade Count:2 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.74746 - 0.74746 J/cm @Thickness 3.17 - 3.17 mm |
1.4003 - 1.4003 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.747 J/cm Grade Count:2 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 0.74746 - 1.28136 J/cm @Temperature -40.0 - -40.0 °C |
1.4003 - 2.40051 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.85 J/cm Grade Count:3 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Notched | 0.74746 - 1.28136 J/cm @Thickness 3.17 - 3.17 mm |
1.4003 - 2.40051 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.85 J/cm Grade Count:3 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |