Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.534 - 1.87 J/cm | 1.00 - 3.50 ft-lb/in | Average value: 1.25 J/cm Grade Count:44 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® PSU1700 Polysulfone General purpose polysulfone with excellent clarityAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 0135 BL069 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF/B40 L 20% Glass Bead/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by Weight and Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation .. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM CO TL20 LE Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® SUG30 ABS Glass fiber reinforced, high heat resistant and flame retarded ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by P.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N140MGHSL (DAM) Nylon 6, 40% Mineral/Glass Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Washington Penn High Modulus Polypropylene Copolymer 15% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ISO 180/A |
CTC X-PRO CTC PP 2040 Polypropylene Copolymer X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Aaron Industries AVPS GP(crystal) 100-1 Virgin Polystyrene - Crystal Melt flow index may be specified. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436T30L Talc Reinforced |
|||
Izod Impact, Notched | 0.534 - 1.07 J/cm | 1.00 - 2.00 ft-lb/in | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 4007 XGS Polypropylene Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase |