Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.368 J/cm | 0.690 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Hostacomâ„¢ 63A6-4 Polypropylene Homopolymer Description: Hostacomâ„¢ 63A6-4 medium high melt flow, 2,200 MPa flexural modulus, 40% calcium carbonate-filled polypropylene homopolymer has an excellent combination of properties, chemical resi.. |
|||
Izod Impact, Notched | 0.368 J/cm | 0.690 ft-lb/in | ASTM D256-10A |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |