Polymer Property : Izod Impact, Notched = 0.410 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.219 J/cm
0.410 ft-lb/in
Asahi Kasei Thermylene® P-30TC-1156 Chemically Coupled Polypropylene Compound, 30% Talc Filled
Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei
Izod Impact, Notched 0.219 J/cm
0.410 ft-lb/in
Abatron AboCast 50-16/AboCure 50-12 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours..