Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.500 - 4.30 J/cm | 0.937 - 8.06 ft-lb/in | Average value: 1.82 J/cm Grade Count:9 |
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and .. |