Izod Impact, Notched 0.750 - 1.50 J/cm
1.41 - 2.81 ft-lb/in
Average value: 1.05 J/cm Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Notched 0.450 - 1.50 J/cm

@Temperature -40.0 - 0.000 °C
0.843 - 2.81 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.579 J/cm Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.550 - 1.50 J/cm
1.03 - 2.81 ft-lb/in
Average value: 1.04 J/cm Grade Count:4
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Izod Impact, Notched 0.900 - 1.50 J/cm
1.69 - 2.81 ft-lb/in
Average value: 1.18 J/cm Grade Count:4
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Izod Impact, Notched 1.30 - 1.50 J/cm
2.44 - 2.81 ft-lb/in
ASTM D256
Loxim 130 01HB Polycarbonate, 30% Glass Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 1.30 - 1.50 J/cm
2.44 - 2.81 ft-lb/in
ASTM D256
Loxim 130 01V0 Polycarbonate, 30% Glass Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.380 - 1.50 J/cm

@Temperature -40.0 - -20.0 °C
0.712 - 2.81 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.940 J/cm Grade Count:1
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..