Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.588399 - 1.49492 J/cm @Temperature -30.0 - -20.0 °C |
1.10231 - 2.80060 ft-lb/in @Temperature -22.0 - -4.00 °F |
Average value: 0.752 J/cm Grade Count:5 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Izod Impact, Notched | 0.588399 - 1.49492 J/cm @Thickness 3.17 - 6.40 mm |
1.10231 - 2.80060 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 0.752 J/cm Grade Count:5 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |