Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.420 - 1.28 J/cm | 0.787 - 2.40 ft-lb/in | Average value: 0.679 J/cm Grade Count:53 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.214 - 1.28 J/cm | 0.400 - 2.40 ft-lb/in | Average value: 0.364 J/cm Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Notched | 0.160 - 1.28 J/cm | 0.300 - 2.40 ft-lb/in | Average value: 0.506 J/cm Grade Count:27 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.427 - 1.28 J/cm | 0.800 - 2.40 ft-lb/in | Average value: 0.843 J/cm Grade Count:34 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 1.07 - 1.28 J/cm | 2.00 - 2.40 ft-lb/in | ASTM D265 |
Alcoa KAMA 3200 Prime High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea.. |
|||
Izod Impact, Notched | 0.801 - 1.28 J/cm | 1.50 - 2.40 ft-lb/in | Average value: 0.949 J/cm Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |