Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.370 - 0.590 J/cm @Thickness 6.35 mm |
0.693 - 1.11 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.270 - 0.590 J/cm | 0.506 - 1.11 ft-lb/in | Average value: 0.413 J/cm Grade Count:3 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Izod Impact, Notched | 0.370 - 0.590 J/cm @Thickness 6.35 mm |
0.693 - 1.11 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.430 - 0.590 J/cm @Thickness 6.35 mm |
0.806 - 1.11 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.260 - 0.590 J/cm @Temperature 0.000 - 0.000 °C |
0.487 - 1.11 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.330 J/cm Grade Count:2 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.260 - 0.590 J/cm @Thickness 6.35 - 6.35 mm |
0.487 - 1.11 ft-lb/in @Thickness 0.250 - 0.250 in |
Average value: 0.330 J/cm Grade Count:2 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |