Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 7746 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 7746 A HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 7.15 J/cm | 13.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 7.15 J/cm @Temperature 23.0 °C |
13.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied.. |
|||
Izod Impact, Notched | 7.15 J/cm @Temperature 0.000 °C |
13.4 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |