Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.48 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2289 PC Lexan* LUX2289 resin is an injection molding grade with high light reflectance |
|||
Izod Impact, Notched | 6.48 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
Izod Impact, Notched | 6.48 J/cm @Thickness 3.17 mm |
12.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC-1212FRO Natural, Flame Retardant Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |