Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.61 J/cm @Thickness 3.17 mm |
10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Izod Impact, Notched | 5.61 J/cm | 10.5 ft-lb/in | ASTM D256A |
Dow INSPIRE™ 117.00 Performance Polymer 117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity a.. |
|||
Izod Impact, Notched | 5.61 J/cm | 10.5 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C20L Calcium Reinforced |
|||
Izod Impact, Notched | 5.61 J/cm | 10.5 ft-lb/in | ASTM D256 |
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded .. |