Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.04 J/cm | 5.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
Izod Impact, Notched | 3.04 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
5.69 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 3.04 J/cm | 5.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 3.04 J/cm | 5.70 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 3.04 - 4.11 J/cm | 5.70 - 7.70 ft-lb/in | |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Izod Impact, Notched | 3.04 J/cm | 5.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 3.04 J/cm | 5.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |