Mechanical Properties Metric English Comments
Izod Impact, Notched 1.95 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
3.65 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Izod Impact, Notched 1.95 J/cm
3.65 ft-lb/in
ASTM D256
Solvay TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY
Description: Polyamide 6, reinforced with 11% of glass fiber, with high impact resistance, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® C 246SI V11 has good mech..