Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 type "A" |
Technetics Group Amicon™ PVDF
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
KYDEX® 6200 Thermoplastic Sheet Fire rated sheet for mass transitApplications: Dashboards, seatbacks, armrests, tray tables, window reveals, cabin linersFeatures: Kydex 6200 is a proprietary, high performance thermoplastic sheet. .. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256-93a |
Multibase Multi-ABS 3832 Natural Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than n.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF15 50100 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature -28.9 °C |
3.50 ft-lb/in @Temperature -20.0 °F |
ASTM D256 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 X 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composit.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: UV Stabilizer, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Good UV.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.17 mm |
3.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN133GL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Westlake Plastics Propylux® CN-P Polypropylene (conductive) Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 32°F; ASTM D256A |
Dow DT702 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Engineered Polymer Solutions ABS PCR 400, Recycled General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 990L-50G Nylon 610, 50% Glass Reinforced 50% glass reinforced, excellent dimensional stability and low water absorption. Also available as: 990LS-50G, same with heat stabilizer.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.87 J/cm @Diameter 3.17 mm |
3.50 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 6260 Super High Impact Polystyrene
(discontinued **) Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined.. |