Polymer Property : Izod Impact, Notched = 1.53 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.53 - 3.2034 J/cm

@Temperature -40.0 - -30.0 °C
2.87 - 6.0013 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 2.37 J/cm Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Izod Impact, Notched 1.53 J/cm

@Temperature 23.0 °C
2.87 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Flint Hills AP6835-HS Polypropylene Impact Copolymer
Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource..
Izod Impact, Notched 1.53 J/cm

@Temperature -30.0 °C
2.87 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Izod Impact, Notched 1.53 J/cm

@Temperature -30.0 °C
2.87 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Valox® 357 PBT+PC
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Izod Impact, Notched 1.53 J/cm
2.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66
LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow.