Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.219 J/cm | 0.410 ft-lb/in | |
Asahi Kasei Thermylene® P-30TC-1156 Chemically Coupled Polypropylene Compound, 30% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.219 J/cm | 0.410 ft-lb/in | |
Abatron AboCast 50-16/AboCure 50-12 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/14 ratio. Pot life: 500 g, 38 min. at 25°C (77°F). Exothermic Peak 280°C (535°F). Hardens in 2-24 hours.. |