Polymer Property : Izod Impact, Notched = 0.187 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CA - 75 LL General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 81 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 82 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 82 UVA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 86 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 75 HID General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 80 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Temperature 23.0 °C
0.350 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy
Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPS 80-0201 Crystal Polystyrene
Description: Injection Molding Grade, High Heat ResistantInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 75 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 81 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
0.125 in; ASTM D256
M. Holland Company GS411 Polystyrene  (discontinued **)
Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio..
Izod Impact, Notched 0.187 - 0.694 J/cm
0.350 - 1.30 ft-lb/in
Average value: 0.388 J/cm Grade Count:4
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
ASTM D256
Ineos H12E-00 Polypropylene Homopolymer, Antistatic
An antistated polypropylene homopolymer produced by Ineos utilizing catalyst technology.It is designed for injection molding and general purpose extrusion. This material meets the Food and Drug Adm..
Izod Impact, Notched 0.187 - 0.320 J/cm

@Temperature 23.0 °C
0.350 - 0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ineos H20Z-03 Polypropylene Homopolymer
This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520...
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
ASTM D256
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o..
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® PPH100-12M Polypropylene Homopolymer
Information provided by Chase Plastics.
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
1/8 in.; ASTM D256
Chevron Phillips MC3700 High Flow Crystal Polystyrene
DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 75 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 75 UVA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 80 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 82 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Copyright © lookpolymers.com All Rights Reserved