Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 - 0.900 J/cm² | 2.38 - 4.28 ft-lb/in² | Average value: 0.765 J/cm² Grade Count:11 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.100 - 0.900 J/cm² | 0.476 - 4.28 ft-lb/in² | Average value: 0.325 J/cm² Grade Count:6 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.600 - 0.900 J/cm² @Temperature -30.0 - -20.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.713 J/cm² Grade Count:8 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact, Notched | 0.600 - 0.900 J/cm² @Temperature -30.0 - -30.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.750 J/cm² Grade Count:4 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |