Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 0.550 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 2.62 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.440 J/cm² Grade Count:6 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.195 - 0.550 J/cm² | 0.928 - 2.62 ft-lb/in² | Average value: 0.341 J/cm² Grade Count:20 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact, Notched | 0.440 - 0.550 J/cm² @Temperature -30.0 - -30.0 °C |
2.09 - 2.62 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.495 J/cm² Grade Count:2 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Charpy Impact, Notched | 0.350 - 0.550 J/cm² | 1.67 - 2.62 ft-lb/in² | ISO 179 |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact, Notched | 0.450 - 0.550 J/cm² | 2.14 - 2.62 ft-lb/in² | ISO 179 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |