Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.27 J/cm² @Temperature 23.0 °C |
6.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG30-FH00B1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.27 J/cm² @Temperature -30.0 °C |
6.04 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Charpy Impact, Notched | 1.27 J/cm² | 6.04 ft-lb/in² | |
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Charpy Impact, Notched | 1.27 J/cm² | 6.04 ft-lb/in² | |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |