Polymer Property : Charpy Impact, Notched = 54.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 11.5 J/cm²
54.7 ft-lb/in²
Partial Break; ISO 179-1/1eA
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data)
TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C.
Charpy Impact, Notched 11.5 J/cm²

@Temperature -30.0 °C
54.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Charpy Impact, Notched 11.5 J/cm²
54.7 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® BFZ 3 PA6
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril..
Charpy Impact, Notched 11.5 J/cm²
54.7 ft-lb/in²
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Charpy Impact, Notched 11.5 J/cm²
54.7 ft-lb/in²
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r..