Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.21 J/cm² @Temperature 23.0 °C |
5.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.21 J/cm² @Temperature -30.0 °C |
5.76 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Charpy Impact, Notched | 1.21 J/cm² | 5.76 ft-lb/in² | |
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |