Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.630 J/cm² @Temperature 22.8 °C |
3.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature 22.8 °C |
3.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature 22.8 °C |
3.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature 22.8 °C |
3.00 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature 23.0 °C |
3.00 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergamid™ B700 Mi10 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.630 - 1.89 J/cm² | 3.00 - 8.99 ft-lb/in² | Average value: 1.19 J/cm² Grade Count:9 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature 23.0 °C |
3.00 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Charpy Impact, Notched | 0.630 J/cm² | 3.00 ft-lb/in² | ISO 179 |
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Charpy Impact, Notched | 0.630 J/cm² @Temperature -20.0 °C |
3.00 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
IRPC Polimaxx Polene 2500H Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT HIGH IMPACT, HIGH TOUGHNESS GOOD EXTRUDABILITYAPPLICATIONS: SHEET / BLOW MOLD EXTRUSION AND INJECTION MOLDING FOR CORRUGATE SHEETS, SHEETS FOR FILE, HOUSEWARES, CONTAINERS.. |
|||
Charpy Impact, Notched | 0.630 J/cm² | 3.00 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® CRN7015 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.630 J/cm² | 3.00 ft-lb/in² | EN ISO 179/1eA |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Charpy Impact, Notched | 0.630 J/cm² | 3.00 ft-lb/in² | EN ISO 179/1eA |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Charpy Impact, Notched | 0.630 - 1.40 J/cm² | 3.00 - 6.66 ft-lb/in² | Average value: 0.826 J/cm² Grade Count:8 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |