Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179 |
GEHR Plastics PP-30PET-F Polypropylene, 30% PET Fiber Reinforced
(discontinued **) Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle... |
|||
Charpy Impact, Notched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant. |
|||
Charpy Impact, Notched | 5.10 J/cm² | 24.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Charpy Impact, Notched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 5.10 J/cm² | 24.3 ft-lb/in² | ISO 179-1 |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |