Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.13 J/cm² | 10.1 ft-lb/in² | |
Ineos ABS Centrex® 821 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection .. |
|||
Charpy Impact, Notched | 2.12 J/cm² | 10.1 ft-lb/in² | |
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **) 16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 2.13 J/cm² | 10.1 ft-lb/in² | |
Ineos ABS Centrex® HGM ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |